Wednesday, May 18, 2011

[MW:11078] Hydrotesting of unfired pressure vessel

 

Hi,all


One of our 3rd party inspector refused to witnessed hydro test of unfired pressure vessel because the actual site erection of vessel is vertical but we offered vessel Hydro at horizontal due to space restriction. vessel diameter 3000mm X 3200 mm longx12 mm thickness.


Construction code ASME section IX.


What is the reason behind the position in doing Hydro test,what will be effect/reason for rejection if the vessel was tested in horizontal position and any standard says regarding this condition.


Pl. suggest.



Regards,


K. Venkateswaran

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...