Dear All,
I like a little knowledge about P91 seamless pipe heat treatment. As
per standard its says Normalizing ans tempering. Please guide about
that what should be cooling media and cooling rate on both the
condition when the job thickness is 38 & 30 mm.
Regards--
Sandy
UAE
I like a little knowledge about P91 seamless pipe heat treatment. As
per standard its says Normalizing ans tempering. Please guide about
that what should be cooling media and cooling rate on both the
condition when the job thickness is 38 & 30 mm.
Regards--
Sandy
UAE
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.