Wednesday, July 21, 2010

Re: [MW:6061] Dual certification of material- valve & pipe- SS316/316L ??

yes
On 7/21/10, Rana Vikas <vhrana@gmail.com> wrote:
> Thanks you.
>
> Does mill provide dual certify materials ???
>
> On Wed, Jul 21, 2010 at 8:28 PM, Raghuram Bathula <raghurambathula@gmail.com
>> wrote:
>
>> simplest way is carbon content as per 316L grade and UTS/YS as per 316
>> grade will meet both the requirements.
>>
>>
>> On Wed, Jul 21, 2010 at 5:17 PM, Rana Vikas <vhrana@gmail.com> wrote:
>>
>>> Dear All,
>>>
>>> Can you inform meaning of dual grate certification material ??
>>>
>>> Also send properties of SS316/316L
>>>
>>> One of our client specification mentioned that piping & valve material
>>> should be dual certified i.e SS316/316L .
>>>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...