Sunday, February 23, 2025

Re: [MW:35446] Filler wire for welding off SA182F11 to SA268TP446

Dear Mr. Sujit Kumar,
The details are sourced from Welding handbooks.
I am enclosing a part of it for your records.
rgds,
C S
---------------------------------------------------------------------

On Thu, 20 Feb 2025 at 12:53, sujit kumar <sujitkumar19942@gmail.com> wrote:
Hello Sridhar,

Thank you so much for your response.
May I know the source how you have selected that filler wire for SA182F11 to SA268TP446 welding....if you have any document regarding that could you please share that document. I will be grateful to you.



Thanks and regards
Sujit kumar

On Fri, 14 Feb 2025, 05:51 sridhar cn, <sridharcn305@gmail.com> wrote:
ERNiCr-3 (Inconel 82)  for corrosion resistance or  ERNiCrMo-3 (Inconel 625)  for corrosion resistance 
and extreme environments, or ER309L  for general purpose could be used.
Preheating  & interpass temp. control will help  to minimize the risk of cracking.  PWHT might be necessary 
to relieve stresses and improve the weld properties.
Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------


On Thu, 13 Feb 2025 at 18:41, sujit kumar <sujitkumar19942@gmail.com> wrote:
Hello experts

Greetings for the day.


Kindly please tell me what will be the filler wire for welding of
SA182F11 to SSA268 TP446




Best regards
Sujit kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKQrt%2Ba3WvcLqQNQA%2BWW6KBw649UUC_Nh2xdcpwHPhzw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihKtTvsp_3w__4-ZEpwG-YJCumSn%3DABrjWQ-N2%2BD3Q5NQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWOngx4uRU1nAKmYj5bpK6CimrzoTX-ur9wFw5uhPvmyXA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiigwv6Uf5VhYHXbbBdv_aWsf5%3DUFk7LB%2B9WcqbiFjjyzA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...