Thursday, February 13, 2025

Re: [MW:35436] Weld overly WPS PQR Qualification on carbon steel material (SA266) with SDSS


SA 266 + TYP309MO  overlay 
then PWHT 
THEN  DP test 

Then TYPE 2594  overlay 

Do overlay as per thickness requirements 

Then DPT
Then machining as per drawing 

ThenDPT

VISHWAS
IWE
Sent from my iPhone

On 11 Feb 2025, at 10:23 PM, Aniruddh Chaudhary <aniruddhchaudhary75@gmail.com> wrote:

Dear Experts, 

Please give your expert advice to stabilise new  WPS/ PQR  for below:

* SDSS Weld overly on carbon steel material (SA266) with PWHT


Regards 

AK Chaudhary 




 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAAs86OtY6iT4WPMQYfkD6JDwpkL8W011ZoD%2ByaCj2M6BPnMa_w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...