The points to be included in the "Notes" section of Form U-1A depend on the type of vessel (e.g., cryogenic, NACE, or lethal service) and the material used (SS, Duplex, or Carbon Steel). Below are the common points to consider:

Common Points to Include in U-1A Notes:

1. Radiographic Examination (RT)

Percentage of the vessel subjected to RT (e.g., "Shell and heads 100% RT per UW-11(a)").

Acceptance criteria (e.g., "RT per ASME Section VIII, Div. 1, UW-51").


2. Post Weld Heat Treatment (PWHT)

If applied, mention the temperature and holding time (e.g., "PWHT at 1150°F for 1 hour per UCS-56").

If exempted, state the exemption clause (e.g., "PWHT not required per UCS-56(d)").

3. Impact Testing

If required, reference the applicable impact test exemption rules (e.g., "Impact tested per UG-84" or "Exempted per UCS-66").

4. Material Certification

If material traceability applies, note it (e.g., "All materials comply with ASME Section II, Part A and B").

Mention any dual-certified materials (e.g., SA-516 Gr. 70 / SA-515 Gr. 70).

5. Special Service Conditions (if applicable)

If designed for cyclic service, reference U-2.

6. Design Code & Special Considerations

Mention any Code Cases used.

Any Finite Element Analysis (FEA) carried out for specific weld joints.

Type of Bolt, Stud, and Washer used.

Best regards,
Deerendra
+91-9112146005

On Sun, 9 Feb, 2025, 19:49 israr, <ahmedisrar.nm@gmail.com> wrote:
Dear Team,
Could anybody tell what specific points to write in Notes of form U-1A?
Our AI always change the points every time.


On Friday, February 11, 2011 at 10:38:54 AM UTC+5:30 Prasad wrote:
Dear experts & ASME Authorized Inspectors,


Our company have ASME certificate of authorization for ASME U stamp
with scop covering
manufacturing activities at shop & field sites controlled by our
company.
We have constructed a pressure vessel at field site owened by our
customer.
Now we have to prepare MDR in U1 form.
My question is againest name & address of manufacturer whether we have
to put field site address or address of our company as apeared on
certificate of authorization.

Please share your experience & views on above.

Thanking you.

Prasad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ee319b7c-bfad-49a4-b12d-66970c6653f8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9GAi7uQeke%2B_qSue_NOQEGq%2BhKQbmKm9c_33yPMSdMbdg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...