Thursday, February 13, 2025

[MW:35428] Welding Qualification for Shell with Rod full Penetration Welding


Capture.PNG
Dear Friends,

Can you suggest me for a welding qualification for the above joint detail.

Material : Shell - SA 516 Gr.70
Rod : Duplex
Welding process: GTAW + SMAW

In my point of view, Plate to plate (Dissimilar) normal butt welding WPS & PQR is enough.  

Why I have a doubt is, here there is Diameter for Rod. So is there any Special Welding qualification for including the Diameter.

Please provide me the full step of Welding Qualification for the above Joint detail.


Regards,
A.Shivasankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c21ac9de-5d5f-4b97-91fd-882f63069a4bn%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...