Re: [MW:35405] WPS for Furnace PWHT

For Furnace PWHT, All Joints under Heating and Cooling Cycle of Heat Treatment, How to ensure it's joint behaviour if not used WPS with PWHT!


On Mon, 27 Jan 2025, 13:20 Vishwas Keskar, <vvkeskar123@gmail.com> wrote:
Pl elaborate your query 
Query is not clear 
Sent from my iPhone

On 27 Jan 2025, at 11:57 AM, Prakash Kumar Bontra <prakashbontra@gmail.com> wrote:


For furnace PWHT as per ASME B 31.3 all the joints in the spool (1" to 36") need PWHT approved WPS and where to refer?

Prakash Bontra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANeLWoNy0URXS9X7TEvvZRVe4V-1LNPKwidHJ097fDyPAjyh7Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/9C99E29D-02AE-4D96-87E5-8B83DEE92269%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACbJsY%2BpYojdoJ_azHw2vKYg2BYe8RHCLXDBdQsbHfz42AqJ4w%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...