Re: [MW:35406] WELDING PRECAUTIONS

why do u want to use inconel 625, instead u can use 321 itself , since u r using TIG there will not be much issues with 321 filler wire. 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Fri, Jan 24, 2025 at 10:28 PM Ch Bilal jovinda <chbilaleng1989@gmail.com> wrote:

Dear Experts,

I seek your guidance on the following query:

When welding SS 312 TP 321H material using the GTAW process with ERNiCrMo-3 filler metal, what are the major safety precautions required to control the cooling rate to avoide sensitization?

Your valuable insights will be highly appreciated.

Best regards,,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAOq7hqvvAnhZe_2t48vM1SKc-p6i6g_1ENr%2BC7%2BOF6Z_rRAFZw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePB%2BcPQ%2BpRfe3Xnnu0MMy0sOkPUDG%2BfX0r2urCdiF0MyA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...