Bevel angle, backing for SMAW Process is not a essential variable for WPS , so no need new WPS.
On Thu, 6 Feb 2025, 8:51 am Zeenathunnisa Kabeer Ahamed, <zeenathk0101@gmail.com> wrote:
Dear sir,--I am having Two clarifications In welding.Kindly clarify the same.1. Including angle 60deg (groov weld butt joint)already we are having wps and pqr. For 45deg Angle with backing plate seperate wps required or not.2. Tensile and bend test will be done along with backing strip or withoout backing strip.Thanks and RegardsS.M.kabeer AhamedSenior EngineerQuality evaluation and systems team pvt Ltd.Bangaluru.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKZhX5sU1QyiPt9e6wuDVnkfmRt0225M_WOB%2BUsSbtxSjQ%3D%2BxA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyK%3DvrgOfTcMhykG1Zb-rj9w%3DrGnavicB2hj%3Dp%2B_U7k9m_Q%40mail.gmail.com.