Re: [MW:35434] Welding sequence plan

A welding sequence plan is a structural approach to performing welds in a specific order to control heat 
distribution, and esure the structural integrity of the welded components. It is commonly used in fabrication, 
construction, and manufacturing industries.

The key component of a welding sequence plan:
1. Welding order: Specifies the sequence in which welds should be performed,
2. Weld Type & Process. Defines the welding method (e.g., SMAW, GMAW, GTAW etc.) and joint configurations,
3. Preheating & Post-weld Treatment: Indicates if preheating or stress-relieving procedures are needed,
4. Clamping & Fixting: Details how to hold parts in place to prevent its movement during welding,
5. Heat control & Distortion prevention: Includes techniques such as backstep welding  intermittent welding, or 
    symmetrical welding,
6. Inspection & Quality: Outlines checkpoints for verifying weld quality through  visual or non destructive and 
    Destructive methods.

Welding sequence plan is important to:
1. Minimises distortion: Proper sequencing distribues heat energy.
2. Prevents Warping & residual stress: Reduces internal stresses that may weaken  the structure.
3. Ensure consistency: Helps maintain welding standards and avoids defects.
4. Improves deficiency: Reduces rework and speeds up the fabrication process. 
Trust it is clear.
C Sridhar.
---------------------------------------------------------------------------------------------------------------

On Tue, 4 Feb 2025 at 10:35, quang anh nguyễn <nguyenquanganh.hp123@gmail.com> wrote:
Dear All.
I am a new member and a recent graduate. I would like to get some advice on  WELDING SEQUENCE PLAN. References would be great.
Thank You

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/150f403e-f349-4329-a1bc-ebee9482f676n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYiiZjLfGEDz4cLWvOKBg%3DEP-13zRoHPYiB1-Hdg%2BhOz_MQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...