Both codes are not identical,
Both codes having separate formats. Mechanical testings tensile and bend test same for both codes. So after testing you can write WPS for ASME and PED separate.
Regards
D.V.Reddy
On Sat, 15 Feb 2025, 11:06 am israr ahmed, <ahmedisrar.nm@gmail.com> wrote:
Can anybody suggest if we can prepare a asme ix wps based on the test carried out as per iso 15614-1?--On Fri, 14 Feb, 2025, 6:06 pm , <materials-welding@googlegroups.com> wrote:
sujit kumar <sujitkumar19942@gmail.com>: Feb 13 08:33AM +0300
Hello experts
Greetings for the day.
Kindly please tell me what will be the filler wire for welding of
SA182F11 to SSA268 TP446
Best regards
Sujit kumar
sridhar cn <sridharcn305@gmail.com>: Feb 13 11:00PM +0530
ERNiCr-3 (Inconel 82) for corrosion resistance or ERNiCrMo-3 (Inconel
625) for corrosion resistance
and extreme environments, or ER309L for general purpose could be used.
Preheating & interpass temp. control will help to minimize the risk of
cracking. PWHT might be necessary
to relieve stresses and improve the weld properties.
Sridhar.
-------------------------------------------------------------------------------------------------------------------------------------
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEJozaJHmQHhU37qEZz-L2FrKMP1JtzMw%3DJbjYTU%2BjtGZ5SCYA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKnKc6xm4xGLu47YRSUnc0VnkD7Ve0f18nOXQUDPbyDycw%40mail.gmail.com.
Comments