[MW:35435] Weld overly WPS PQR Qualification on carbon steel material (SA266) with SDSS

Dear Experts, 

Please give your expert advice to stabilise new  WPS/ PQR  for below:

* SDSS Weld overly on carbon steel material (SA266) with PWHT