With attached code ref. you can use EN ISO 15614-1 WPQR test results for preparation of WPS/PQR as per ASME BPVC Sec. IX.
Thanks.
Best Regards,
Navanath Kashid
International Welding Engineer (IWE-IIW)
Mob. No. 9665851969
On Sat, Feb 15, 2025 at 6:05 PM <materials-welding@googlegroups.com> wrote:
israr ahmed <ahmedisrar.nm@gmail.com>: Feb 15 11:02AM +0530
Can anybody suggest if we can prepare a asme ix wps based on the test
carried out as per iso 15614-1?
venkateswara reddy Desireddy <dvreddy82@gmail.com>: Feb 15 01:23PM +0530
Both codes are not identical,
Both codes having separate formats. Mechanical testings tensile and bend
test same for both codes. So after testing you can write WPS for ASME and
PED separate.
Regards
D.V.Reddy
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2B8p7iW5K5iBizc3qePAL4x6mGG9HnV-DaX7juJAL%3Dr_J0sCng%40mail.gmail.com.
Comments