Re: [MW:34607] Dissimilar welding chemical/PMI acceptance criteria

Dear Sir,
As per ASTM B474, Chemical analysis of weld shall match the chemistry of ERNiCrMo-3, in case of dilution effect manufacture and purchaser agreement is required,
Here, weld chemistry is matching the alloy 825, Is it acceptable?

Regards,
Manish Tripathi
On Tuesday, 24 October, 2023 at 9:31:36 pm UTC+5:30 Vishwas Keskar wrote:
Chemical analysis of the weld joints in not a mandatory test  in any Code  either in similar or dissimilar welds.
Some Customer specifications are imposing it .
You have to give ref of the dilution phenomenon and communicate the details to QAC 

There is dilution. So weld metal chemistry will be not exactly as per filler wire due to dilution effect .

Additional one - Chemical analysis is mandatory in case of corrosion overlays - Undiluted Chemistry at the depth   
Thanks
Vishwas- IWE

 

Sent from my iPhone

On 24-Oct-2023, at 6:42 PM, Manish Tripathi <manish.tri...@gmail.com> wrote:

Dear Experts, 
Please provide reference of CODE, for chemical analysis acceptance of dissimilar welding. Here Alloy 825 welding by ERNiCrMo-3, 
Ideally weld metal should match ERNiCrMo-3, But can we accept Alloy 825 chemistry in weld metal.

Welding Process: EFW
Design Code: ASME Sec VIII Div.1
Welded part: Pipe Long Seam ASTM B474.

Regards,
Manish Tripathi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc840d34-c98a-4419-9685-52e8df7196e6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/61d00682-6f97-468a-b8d2-c73e6fb8d224n%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...