Monday, June 19, 2023

Re: [MW:34347] Impact test requirements

Der Jithin,

Since your coupon thickness is 9.53mm, make sure your impact specimen is 7.5 mm. if your 2nd process Gtaw is covering in this 7.5 mm, separate specimen is not required.

On Mon, Jun 19, 2023 at 7:46 AM JITHIN GOPINATH <2k9jithin@gmail.com> wrote:
Sir,
   I am qualifying a PQR with the process GMAW+SMAW with 9.53mm thickness.
I want to do impact test at -25degree C, so someone please advise me  should I take impact test specimen for each process, means a separate specimen for GMAW and SMAW required or I can take a single specimen for the test.
Qualification code API 1104



Regards 
Jithin 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAT3KQ5%2B6n69y7Ln1OVVSxxjOfGHAAyW3PQywQiWHyOV4Ms%3DKQ%40mail.gmail.com.


--
Thanks & Regards,
 
Srinivasrao.Gundala,

Please consider your environmental responsibility: before printing this e-mail, ask yourself whether you need a hard copy!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACn7QWXRPVJjp%2BgR%2BRwaJR-5ma4BsOrUcKpj73jmEyTanOoaVA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...