Re: [MW:34298] Impact test requirement for Unlisted material (ASTM A707 L5 CL3)

Base metal thickness qualified is 16mm to 50.4mm


On Mon, 12 Jun 2023 at 11:54, aravind roche
<aravindroche@gmail.com> wrote:
Thanks for your all response, 
we done the impact at -55°C in PQR, My query is our service fluid is water and service temp is 0° to 90°C, i believe then the thickness range in WPS we can use 5 mm to 50.4 mm.  
Design Code: B31.3
Qualification Standard : ASME Sec IX

On Monday, June 12, 2023 at 6:06:35 AM UTC+3 james gerald wrote:
ASTM A707 L5 forged product material impact tested at -60degC But API 5L X65  material for a thickness of 50.8 require Impact tests as per ASME B31.3 and hence PQR shall be impact tested

Thanks & Regards

J.Gerald Jayakumar

0091-8838619635



On Saturday, 10 June, 2023 at 05:37:53 pm IST, aravind roche <aravin...@gmail.com> wrote:


Experts,

please advise below,  I believe because of our service temperature the impact test is not required, please guide me. 

PQR material - A707 L5 CL3 to API 5L Gr X65
Thickness coupon: 25.4 mm
WPS qualified range is : 5 to 50.8 mm
Design code : B31.3
Qualification Standard : ASME Sec IX
Our Project MDT : 0° to 90°C
Service : Water
PWHT : Yes
Pre heat : Yes

Aravind.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/7560590a-02d8-4cdc-931e-db926a941addn%40googlegroups.com
.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/198856590.1550546.1686551419313%40mail.yahoo.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...