[MW:34269] Flux didn't Peel off

Hello Everyone,

Hope all are doing well,

I have to ask in SAW welding Flux did not peel off. 
F7A4-EM12K

What to do about it?

What precautions should be taken?



Thanks and Regards 

Prabhu

--