Dear Sir, 

1. You can use E-7018-1 

On Thu, Jun 8, 2023 at 11:57 AM Mahesh Rajpurohit <rajpurohitmahesh303@gmail.com> wrote:
Dear Team 

Kindly suggest me the welding rod material standard used S355 J2 N plate 

And method of welding which is suitable for making round pipe from plate of 25mm Thickness 

Your's 
Mahesh Purohit



On Thu, 1 Jun 2023, 08:28 paresh patel, <pareshprod03@gmail.com> wrote:
You can prepare WPS for SMAW only. considering essential variables.


On Tue, May 30, 2023, 4:58 PM QA/QC <adnanziad49@gmail.com> wrote:
Dear master 

please can you advise me i have some doubt 
in our project i have a PQR qualify with gtaw + smaw butt weld 
Detail :
 
7.14 to 20 (CS & LTCS)
GTAW  5 mm +SMAW 9

ER70S-6 + E7018-1 


and i want to qualify to only SMAW PROCESS is it possible or no 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bbac856e-d25b-4408-acbc-6dc6c047506en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAA7RJJPW6QjiQC-irOxERZymO-Su0s2H24%3DwzD3YvKEaRb35dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABQ2pZF%2BDMx2wZ0HZ3VEMWyRiEkhUdTD-LH7kutZwfqs4XxiHQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zevSMgBi9x%2B4cqw%3Dv2-zfR9oC4EmXyfvyrmcGCNcnWvqg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...