Friday, June 9, 2023

Re: [MW:34280] Digest for materials-welding@googlegroups.com - 3 updates in 3 topics

It's regarding Simulation PWHT.

Question- how to prepare 3 cycle Simulation PWHT for SA387 Gr. 11. Low Alloy Steel? 
How to select soaking time and temperature for three cycle. 

Regards, 
Navanath Kashid. 

On Thu, 8 Jun, 2023, 10:23 AM , <materials-welding@googlegroups.com> wrote:
Sunthar Ambikapathy <sunthar1974@gmail.com>: Jun 07 11:32AM +0530

Dear Quality Team,
 
 
 
Pl provide suitable electrodes for as attached PMI composition.
 
 
 
I was selected for the E11018 electrode. With Preheat 150 deg.
 
 
 
What is your option.., and welding procedure ?
 
 
 
Equipment : Air receiver Header ,Size Dia 250mm X 4mm.
 
Application : ESP / Bag filter pulsing header.
 
Services : 12 years old, power plant .
 
Defect: Fillet weld center of portion crack observed.
 
Chinese Power Plant.
 
 
 
 
[image: image.png][image: image.png]
 
 
 
 
--
Kind Regards
 
Sunthar A
+91 9894100888
Shahil Saini <sainishahil98@gmail.com>: Jun 06 07:38PM +0400

Hello everyone,
Good Evening,
hope all are doing well,
 
As my subject indicates PWHT in SS to CS Weld joint, my question is what
are the after effects if pwht performed in SS to CS joint??
 
In Addition, how to mitigate the after effects which occurred after pwht?
 
BM: SS 316L to SA516 Gr.70
Parminder Singh <parmsin2001@gmail.com>: Jun 07 03:32AM -0700

Dear Experts,
 
Will CJP WPS qualify for Fillet Welds ?
You received this digest because you're subscribed to updates for this group. You can change your settings on the group membership page.
To unsubscribe from this group and stop receiving emails from it send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B8p7iWo69OQhr3e6dJawswMr71%3D2NT2_jAtyBVsrLhnsqX7mg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...