Thursday, June 8, 2023

Re: [MW:34277] PWHT on Stainless steel to Carbon Steel Weld

at cs pwht temp, carbide formation??

On Thu, Jun 8, 2023, 12:13 PM Parminder Singh <parmsin2021@gmail.com> wrote:
Buttering of 516 Gr 70 with 309LMo, Then perform PWHT 
then Weld 316L to Buttered CS. 

On Wed, Jun 7, 2023 at 4:28 PM Shahil Saini <sainishahil98@gmail.com> wrote:
Hello everyone,
Good Evening,
hope all are doing well,

As my subject indicates PWHT in SS to CS Weld joint, my question is what are the after effects if pwht performed in SS to CS joint??

In Addition, how to mitigate the after effects which occurred after pwht?

BM: SS 316L to SA516 Gr.70 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALfBO_8bejT55kYnUkJTc5p_DQD7ZRUkb1x%3DRA4u_oNgZTtG0A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zejB7O1YWyqF2-Na5udLVecD_V2sDCsv5e0xxPBGAzfVg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOEMqMfzbFzUztAwuSVA4iGBQ8MJGkuiJfoEMidHebx%3Dg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...