[MW:34319] Welder performance welding repair rate for fillet welds and linear welds

I am making welds for some pipeline projects in which all are linear welds
and some are different joints but all are fillet welds. For all fillet welds, I am having doubt ❓ about the Welder performance weld repair rate as per codes
In SAEP 324 linear is 0.2 percentage
Saes W10 linear is 2.0 percentage
can anyone tell me the exact repair rate percentage in my case as per the code or reference I need to understand the client with reference?

thanks
regards 
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BPrcrLb51mksuGEt%2Byc0i-dK8OVQ7aTf7DVfGJrWs2XWXC9RA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...