Monday, June 12, 2023

Re: [MW:34306] filler wire for Inconel 600

Dear Pham,

Attached table from which Code have taken?

Thanks,

On Mon, Jun 12, 2023 at 3:12 PM Pham Thanh Tinh <tinhamem@gmail.com> wrote:
For your refence 



Vào Th 2, 12 thg 6, 2023 vào lúc 13:19 sujit kumar <sujitkumar19942@gmail.com> đã viết:
Dear all,

What filler wire we have to use to weld 
 INCONEL 600 TO INCONEL 600




Best Regards
sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMr0ieF94PAOgGi0VKuZybuoNmbto1gAXD6M6WspJ2G-g%40mail.gmail.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwbVUAkz8Q4jhLuo65LmEnm5XYDJPnWbeYYncy4s%3Dukjdg%40mail.gmail.com.


--

Regards

Hemant Raychandel

QA/QC Engineer

CPECC

CHINA PETROLEUM ENGG. & CONSTRUCTION CORP. (M.E)

7th Floor, Onyx 2 Office Tower, Greens, Sheikh Zayed  Road, Dubai, U.A.E.

Tel: 04-3837942  |  Direct: 04-3837942  |  Mobile: +971 503316288

Email: hemant.cpecc@gmail.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMVKa9xeGnOz12yE8xDuB%3DmG31N8JHuo2rKBa6fC%2BwcJNBy7gQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...