BS 3100 A2 is supplied in heat treated condition , 

- may be you used ferritic electrode which get high C from CS Base Metal and without heat treatment formed hard phase
- as indicator , what about bend test ? ( free from fissures and small notches in bend faces or have )
 
so , u can check the phase on hard points through its microstructure then decide if weld metal chemical is suitable or need to be modified 

Best Regards ,
ENG. Ahmed Osman



On Thursday, June 8, 2023 at 03:05:07 p.m. GMT+3, 'Saravanan Selvakumar' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Dear All,

A new qualification was made with BS3100 Gr A2 to SS304 pipe welding in 6G position. Hardness value of Weld while testing was found to be 415 and 418 HV10, while in other areas of HAZ, Body where within the range of 175-198 HV10. 

Kindly give your suggestion on why this drastic change in hardness and the acceptance of it.


Regards,
Saravanan S.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3c785ca1-7740-47d5-9931-b3bf99d64088n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...