SMAW-ENICRFE-3
GTAW -ERNICR-3
Thanks & Regards
Dinesh Baskaran
On Mon, Jun 12, 2023 at 3:49 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,--What filler wire we have to use to weldINCONEL 600 TO INCONEL 600Best Regardssujit
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMr0ieF94PAOgGi0VKuZybuoNmbto1gAXD6M6WspJ2G-g%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMAJDVqcwXELd0oVpmSWWyuzTXTLMcaWQGHPJc%3DaXR3Td0MagQ%40mail.gmail.com.
Comments