Saturday, June 10, 2023

Re: [MW:34288] Impact test requirement for Unlisted material (ASTM A707 L5 CL3)

is it so. could u pl give some ref

On Sat, Jun 10, 2023, 6:33 PM Faisal Sattar <faisalsattar315@gmail.com> wrote:
Impact toughness test does not only depend on service temperature only, It also depends on working fluid, for example if your pipeline is sour service then impact toughness test should be conducted fot PQR qualification.



On Sat, Jun 10, 2023 at 4:07 PM aravind roche <aravindroche@gmail.com> wrote:
Experts,

please advise below,  I believe because of our service temperature the impact test is not required, please guide me. 

PQR material - A707 L5 CL3 to API 5L Gr X65
Thickness coupon: 25.4 mm
WPS qualified range is : 5 to 50.8 mm
Design code : B31.3
Qualification Standard : ASME Sec IX
Our Project MDT : 0° to 90°C
Service : Water
PWHT : Yes
Pre heat : Yes

Aravind.A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec3be245-165e-41a9-a0a2-40f333501774n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE%2B-gCa__3VUteHO5R9mYWSATcse57TBr0hvcvMxL2aeWDm39A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNMNTLB-P9aDCZVg5-9aUVnrtbwHkjguvd1dOZbJrQFgA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...