Dear Shahil 
Pl furnish below information :
Why PWHT is required  ?
What is type of joint ?
What is PWHT Holding temperature and Holding time ?
Which type of filler metal that is planed to be used ?
What is service of the equipment ?Corrosive  or Elevated Temp.(If yes what is temp)

Thanks and regards

Vishwas - IWE International Welding Engineer



On Wednesday, June 7, 2023 at 4:28:13 PM UTC+5:30 Shahil Saini wrote:
Hello everyone,
Good Evening,
hope all are doing well,

As my subject indicates PWHT in SS to CS Weld joint, my question is what are the after effects if pwht performed in SS to CS joint??

In Addition, how to mitigate the after effects which occurred after pwht?

BM: SS 316L to SA516 Gr.70 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ff1a54fb-a69f-485f-8463-7905268cc088n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...