Saturday, April 29, 2023

Re: [MW:34163] impact test requirement

Dear vishwas sir,

Please find below reply.


What is the MDMT?----(-45°C @ 10 bar(g))
What is the Welding process?----(GTAW)
What is consumable? ----(ER308L)
Is this consumable is perused tested?( NO NOT TESTED)



Best Regards.
sujit


On Fri, 28 Apr 2023 at 21:44, Vishwas Keskar <vvkeskar123@gmail.com> wrote:
What is the MDMT?
What is the Welding process?
What is consumable?
Is this consumable is perused tested?

 
Go the UHA 51 - There are exemptions to SS consumables .
Pl go thr it .
I am sure these will get exempted 

Thanks 
Vishwas
IWE 


Sent from my iPhone

On 28-Apr-2023, at 4:28 PM, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


1. MDMT
2. Applicable Design code to determine the exemption
3. Welding code such as ASME Sec.IX

Normally supplementary PQR for Hardness and Impact is permitted

Thanks & Regards

J.Gerald Jayakumar



On Friday, 28 April, 2023 at 04:07:48 pm IST, Rameshbabu B <rameshbabu.b@zetwerk.com> wrote:


Impact test temperature?

On Fri, 28 Apr 2023 at 15:44, sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

if we have already qualified WPS for  P no 8 to P no 8 . then now we have  the requirement of the impact test. what to do? since it is a supplementary essential requirement. so may i  prepare test piece for the impact test and attached this impact test report to previous wps...?



Regards.
sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMLtSp8eEQ-4e4NwJTN_PJC72zwr-JSNy5ghOES%3Dwz7VQ%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2keMW%3D8RZdUGKinM%3De3z4W3V82%3DrmXFTwtsw9TtXD85RA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1170775803.711426.1682679001664%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/EE1B29CE-80BE-4DA2-8B0F-9FCC2B50AF20%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPMvdf%3Def75v_yhPSs%3DvE0VuE%2BXs4_92rZrxSa6k0uXrQ%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...