[MW:34161] Re: Suitable Welding Electrodes

For SA333-6 you can utilize the E7018-1
For A350-LF3 E8018-C3 is a good choice
for others, I have to investigate the material properties.

On Thursday, April 27, 2023 at 10:58:49 PM UTC-4 amso...@gmail.com wrote:
  Dear Experts,

Please suggest us the suitable electrode to weld the SA 537 Class1, SA 333 Grade 6, SA350 Gr.LF3 and SA 420 WPL9 with the Impact temperature at -60 Deg.C

Also Shell Thickness of SA 537 Class1 is 12mm & 16mm. Hence is this vessel required PWHT

I have chosen below electrode to weld these materials.

E8018-C3
ER80S-Ni1

E81T5-Ni3C

E81T5-Ni2C

Requesting expert opinions in these regards

Thanks and Regards,

MS


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/5b3f549e-1288-43f9-9305-898fe348db68n%40googlegroups.com.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...