I have to repair / re thread a threaded portion of a 3" control valve seal retainer (Material is SA 479 410SS).
What will be the suitable consumable for this?
Service: Boiler feed water pump outlet.
Size : 3" 1500#
Body: A216 WCB
Thanks & Best Regards
Sanjay