[MW:34123] Suggestion for welding consumable

Dear Experts, 


Kindly suggest consumables for below 


Material SA516GR70

Impact @-40C

Impact values – 27J min

 

Normalizing

Loading – 300C

ROH – 150C

Soaking Temp – 900-920

Soaking Time – 80min

Still Air

 

SR

Loading – 300C

ROH – 50C max/hr

Soaking – 625C- 645C

Time – 720mins

ROC – 65C max / hr upto 425C


Thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8046052f-73a0-46dd-9523-d130fd6069d8n%40googlegroups.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...