Re: [MW:34158] impact test requirement

This will get exempted according to UHA 51.

Still, if you wanted to qualify with an impact test refer below

1. Existing PQR parameters should follow for qualification.
2. Perform an Impact test on the specific temperature and support the results.

Regards

Ramesh Babu Balaram

General Manager - Corporate Quality

84/1, Vaishnavi Sovereign, Green Glen Layout, Bellandur, Bengaluru-560103


M 9840531355 E rameshbabu.b@zetwerk.com  W zetwerk.com

Graphical user interface    Description automatically generated

App Green Footer Image Please consider your environmental responsibility. Before printing this e-mail message, ask yourself whether you really need a hard copy.




On Fri, Apr 28, 2023 at 4:18 PM sujit kumar <sujitkumar19942@gmail.com> wrote:
-50 degree celcius

On Fri, Apr 28, 2023, 16:07 Rameshbabu B <rameshbabu.b@zetwerk.com> wrote:
Impact test temperature?

On Fri, 28 Apr 2023 at 15:44, sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

if we have already qualified WPS for  P no 8 to P no 8 . then now we have  the requirement of the impact test. what to do? since it is a supplementary essential requirement. so may i  prepare test piece for the impact test and attached this impact test report to previous wps...?



Regards.
sujit

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMLtSp8eEQ-4e4NwJTN_PJC72zwr-JSNy5ghOES%3Dwz7VQ%40mail.gmail.com.
--
Regards
Ramesh Babu Balaram
Head QA/QC
Zetwerk Manufacturing Businesses Private Limited
Mobile: +91 98 4 053 13 55

>>>DONATE NOW<<<
SUPPORT ZETWERK'S CAMPAIGN TO FEED THE VURNERABLE MIGRANT FACTORY WORKER POPULATION.
Contribute generously. Each donation will go towards essential ration kits.
Let's come together as a nation so that they don't have to go hungry

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2keMW%3D8RZdUGKinM%3De3z4W3V82%3DrmXFTwtsw9TtXD85RA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWOeQ00qqVJws787WXWCOYcOP9F9k0Q1VdnNk7X%3D%2BGRAAg%40mail.gmail.com.

This information may be confidential and/or privileged. Use of this information by anyone other than the intended recipient is prohibited. If you receive this in error, please inform the sender and remove any record of this message

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHJfB2nbF7Ypkvntj_XxmsxnvHXiO-siLoHWvY4NXDHiw9j%3D%3DA%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...