Tuesday, April 11, 2023

Re: [MW:34126] Procedure for Z test

i donot think Z-Through thickness tensile may not be required for thickness of 16mm.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Apr 3, 2023 at 3:41 PM Prashant Rane <pprane.rane1@gmail.com> wrote:
Check with your testing laboratory for the sample size and testing details

Regards,

On Mon, 3 Apr, 2023, 3:15 pm Dharma dattu, <dharmadattu@gmail.com> wrote:
Dear All,
We have a storage tank to be manufactured . Material is SA516 Gr 70. Thickness of material 16mm.
We have to perform Z test, can you share the procedure.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dc5fa23b-e3e3-40a1-88a0-27696e3405c6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAkMc%3D469WqH%3DAiS5-vi2v4nqNmJb_XHDpMZQ0Y97RbWwdZY3w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eM6LPJFZMJzigwvPAUkfWC9mq6p9WpwVNEdvr4onjwwyw%40mail.gmail.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...