Monday, April 3, 2023

Re: [MW:34113] IMPACT TESTING FOR ASTM A193 L7 MATERIAL STUD

There is no specification as such as ASTM A 193 Gr. L7, Only ASTM A320 L7 exists with Impact test requirement at -101degC

Thanks & Regards

J.Gerald Jayakumar




On Monday, 3 April, 2023 at 01:18:48 pm IST, Mahesh Purohit <marketing@unifitmetalloys.com> wrote:


Dear Sir 

We have an requirement for ASTM A193 GR.L7 stud with impact testing @ -120deg C 

Kindly suggest your best opinion 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ec09c075-4414-4d47-ae2f-b2187ddb7f02n%40googlegroups.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...