Dear Ajay
Yes, you can use the GTAW Process from PQR GTAW+SMAW as long as the essential variable PQR will cover into new WPS.
for thickness range for GTAW Process, refer to Table QW-451.1 of ASME Sect IX, it should be 5mm ~ 14mm
Hopely the above can answer your question
Best regards
Kurniatullah, IWE
On Wed, Apr 12, 2023 at 10:02 AM Ajay Kaipuram <ajaykdas144@gmail.com> wrote:
Hi,I have a PQR with a thickness range of 7mm (GTAW)+ 14.94mm (SMAW) for the groove joint. Can I prepare a new WPS for the job with a 5.08 mm thick groove joint for the GTAW process only? If yes, what thickness range can I mention in the WPS?Regards,Ajay--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b7cd158a-7548-4229-9ead-c6c37bed3548n%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFo4ueq4VobgaLyigwfpRUTSjEyFD32YaWzEkW90DiDhoWvnjw%40mail.gmail.com.
Comments