Please suggest us the suitable electrode to weld the SA 537 Class1, SA 333 Grade 6, SA350 Gr.LF3 and SA 420 WPL9 with the Impact temperature at -60 Deg.C
Also Shell Thickness of SA 537 Class1 is 12mm & 16mm. Hence is this vessel required PWHT
I have chosen below electrode to weld these materials.
E8018-C3
ER80S-Ni1
E81T5-Ni3C
E81T5-Ni2C
Requesting expert opinions in these regards
Thanks and Regards,
MS
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3290864a-54a9-498f-abf2-a682371cc357n%40googlegroups.com.
Comments