Wednesday, April 12, 2023

[MW:34127] USE of PQR of 10.97mm GTAW+SMAW for new WPS GTAW process only

I have a PQR of 10.97mm Test coupon GTAW(3.5mm)+SMAW(7.47mm) in groove Joint, ASME Sec IX . 

Can I prepare a new WPS for GTAW only for the Job with thickness 5.08mm groove joints? If Yes, What thickness range need to be mentioned in the WPS? 5mm to 7mm is Ok?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/03b90f84-3657-431c-8002-d8122e47c3d6n%40googlegroups.com.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...