Thank you for the replies experts.

Wire used: CORDIFF 357 SA (Cr, Ni, and Mo alloyed tubular wire) Make - Diffusion
Flux used: SUPERSHIELD SS Flux Make - Super Alloys and metals (data sheet attached)

Regards,
On Wednesday, 26 April 2023 at 10:37:39 UTC+5:30 RANEESH PK wrote:
because of very  high traveling speed and long weld bead. 

On Wed, 26 Apr 2023 at 7:04 AM Mehrab Chakoshkar <mehrab.c...@gmail.com> wrote:
Hi
First, you should give us sufficient information such as the AWS Classification, the wire and flux name, and the ASTM name of the material.
second, seemingly your welding speed has been high, I can see the long beads in the welding direction.
third, sticking the slag usually happens when the A is too high and the cause of porosity usually is moisture in the flux, have you baked the flux before use?
Mehrab
On Tuesday, April 25, 2023 at 7:40:09 AM UTC-4 SMM wrote:
Dear Experts, 

There are few issues found during SAW weld  cladding at site and are highlighted in the report. Please find attached report.

I have a few questions
1. Reason for such issue to occur. 
2. Is the issue of Flux (neutral basic flux) or Flux cored wire used in the process.
3. Please advise how can this be sorted out.

Thank you,
George

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/19b59249-3500-4de4-beb3-792f09bf2b1fn%40googlegroups.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...