Wednesday, April 12, 2023

Re: [MW:34131] USE of PQR of 10.97mm GTAW+SMAW for new WPS GTAW process only

Thanks Mr. Jayakumar,

The impact test is No Applicable to our job.

Still, I have some doubts about preparing the WPS. Can you please review the area highlighted in the below screenshot? If changes are required, please let me know.

Screenshot 2023-04-12 123448.png

Thanks 

Ajay.



On Wednesday, April 12, 2023 at 6:29:05 AM UTC+3 james gerald wrote:
There are 2 thickness involved, Base metal (BM)Thickness and Weld metal (WM)thickness. Yes, you can prepare a separate WPS for GTAW from the PQR.

When Impact test is Applicable.

BM thickness Qualified,  minimum is 10.97mm so you cannot prepare a GTAW WPS.

When Impact test is not Applicable

BM thickness Qualified,  5mm to 7.0mm (though maximum is 21.94mm)


WM thickness Qualified is maximum 7mm

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 12 April, 2023 at 08:32:52 am IST, Ajay Kaipuram <ajayk...@gmail.com> wrote:


I have a PQR of 10.97mm Test coupon GTAW(3.5mm)+SMAW(7.47mm) in groove Joint, ASME Sec IX . 

Can I prepare a new WPS for GTAW only for the Job with thickness 5.08mm groove joints? If Yes, What thickness range need to be mentioned in the WPS? 5mm to 7mm is Ok?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/03b90f84-3657-431c-8002-d8122e47c3d6n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c5c8e34e-3aae-4746-a4b1-3f8b39370c2cn%40googlegroups.com.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...