Re: [MW:33993] Prequalification of WPS as per AWS D1.1 - PIPE TO PIPE BUTT JOINT(PJP)

Pre Qualifed WPS is available.  Check the joint types 

On Friday, December 16, 2022 at 9:02:01 AM UTC+3 Sandeep wrote:
Dear Sham,


Please refer Fig 5.2 (Page#113 in AWS D1.1:2020 Edition) for the Joint details. Prequalified WPS can be prepared for this joint configuration.

With Regards,

SANDEEP RAGHAVAN

INSPECTION ENGINEER

linkedin icon



On Thu, Dec 15, 2022 at 8:06 AM Sham Shahabuddin -Welding Inspector, HANBO <shamshahab...@gmail.com> wrote:
Dear Experts

Please input your suggestions and comments for my condition below

Joint: Pipe to Pipe corner 45 degrees - Butt 
Size: 4" sch 40 astm A53
Standard: AWS D1.1
Application: Guard Rail
Welding Process: SMAW.

My question is whether prequalified WPS is available for this condition in AWS D1.1 if PJP is used. If available, please let me know with the reference. When I search I'm unable to find any reference with regards to diameter ranges for the prequalified WPS.

image.png
Thanks and Regards
SHAM SHAHABUDDIN
QC INSPECTOR - WELDING

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAyAb6Niu%2B%2BS%3Dq%2BNY-8Tw19WsE6mE7eMTzezyNK-omwwrHCDqg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/00d4d29d-d78f-4a47-ba03-7f35f1287fabn%40googlegroups.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .