Re: [MW:33954] A216M vs A216 material

Dear, 

M indicates Unit of measurement (SI units) please find below abstract  of ASTM A 320- 21a, same Clause may present in A 216 also.

"1.6 This specification is expressed in both inch-pound units and SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI) units, the inch-pound units shall apply."

Regards,
CH V RAMANA 


On Monday, 23 January, 2023 at 12:18:08 pm IST, Michael Tho <michaeltholektong@gmail.com> wrote:


What is the difference between A216 and A216M ?

Normally we offer A216-WCB/WCC however this time the requirement comes with A216M-WCB/WCC.

Please advise and any document that explains the difference?

Thank you.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c6d715aa-ad10-4b7d-8932-821777673ed3n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...