Normally you order Flanges/Pipes/Fittings from the Manufacturer / Stockist with the requirement of EN 10204  3.1/3.2 certified by the manufacturer / TPI who reviews the Normalization chart/graph  in the MDR ( Manufacturer Data Report) and only a statement about Heat Treatment appears in the MTC (as per previous mail)

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 17 January, 2023 at 01:34:07 pm GMT+3, sujit kumar <sujitkumar19942@gmail.com> wrote:


Dear experts,

What is SA105N FLANGE as per ASME SEC VIII DIV 1 .....if normalization is required in that flange then what is the requirement of  MTC. is this required normalization graph at all in that.


regards.
sujit.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/057e3168-af10-49aa-b025-651ac11e85e8n%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...