Thursday, January 12, 2023

Re: [MW:33916] Request for Information

Weld bead width?

On Thu, 12 Jan 2023 at 12:48, Babur Khan <mbabur.bwp@gmail.com> wrote:
Greetings,
Weld bead width or length? 

Muhammad Babur Khan
Sent from my iPhone

On 12 Jan 2023, at 11:19 AM, G Gughan <ggughan17@gmail.com> wrote:


Dear Experts,

It's a very nice platform to gain & share knowledge.

I have a query regarding the weld bead length. What is the maximum weld bead/weave length in Power Piping? (ASME B 31.1)
or 
Is there any thumb rule for weld bead length?

Your idea/advice will be highly welcomed & appreciated.

Be safe & have a healthy Life

Thanks,

Kind Regards,

G.Gughan

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB0bcTMUzgWi-7pQvfdjj-e93ChHhYcq93UYgWC3xe9Kv4hnng%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/508A2E26-370D-4480-BDB4-62F5B6C0097E%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB0bcTMvgi%2BQhSMZTJynWBifU5CcxDDgFMQWFnCDh59xAMVG3Q%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...