F number is a filler material Number specified in ASME Sec.IX. Select correct Fillet material from consumable from manufacturer's catalogue for LTCS material, and refer Table QW 432 of ASME Section IX for F number

Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Monday, January 16, 2023 at 07:41:52 PM GMT+7, ajith asir <asirajith1994@gmail.com> wrote:


Hi Everyone,

I am new to welding engineering. I just want to know the F number, Base material and Process co-relation table. Is there ant details available in Section 9


FNo.png

Thanks
Asir

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb52cf0e-ec11-47be-b05f-c6d2e2838b6an%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...