Saturday, January 14, 2023

[MW:33920] Impact test requirements for PQR

Dear expert's.

We are going to perform PQR  on material API 5L X60 (P1 G2 to P1 G2) 6" pipe.
Thk-21.95mm as per ASME sec 9.
Welding process-(GTAW Er70s-2(spl) + SMAW(E7018-1))


Client requirement are PWHT with impact test with other test as per code .
Kindly guide me for impact test temperature requirements.

We are qualifying this PQR  to weld rolled fittings of A537 CL1. thk 30 mm.
Design code ASME SEC 8 DIV1.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC6cZ-hPkO6LTuoUw2%2BdBnYR1P8ex-Ti9FMwk_OWUr6V681zpA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...