A573 gr 70 12mm
A283 gr C 10mm
On Fri, 27 Jan 2023, 05:21 'james gerald' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
--Also provide the thickness
On Thu, 26 Jan 2023 at 12:23, james gerald<gerry_tup@yahoo.com> wrote:What is the design CODE API 620 / 650
On Thu, 26 Jan 2023 at 12:19, Benaouda Mezrar<mezrarbenaouda4@gmail.com> wrote:But sir we use these two nuances for construction of storage tanks. Is it applicable ? with different thicknesssir please could you give me more arguments about the weldability of these two nuances ?thank you a lot for your helps sir--Le jeu. 26 janv. 2023 à 07:40, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> a écrit :Use E7018 / E7018-1
--On Thu, 26 Jan 2023 at 7:32, Benaouda Mezrar<mezrarbenaouda4@gmail.com> wrote:Dear friendcould anyone answer my question, the question is : could we weld A573 GR70 with A283GR CIn my opinion we can't weld them because the minimum specified tensile arefor A283 GR C = 380 MPAfor A573 Gr70 = 485 MPAPlease friend help me i need this information emergencyif the answer is yes which type of filler metal we should use for SMAW--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20e0e61e-9ee4-4ef3-9080-fe83ae9c39ban%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2043007948.1323331.1674715164817%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANKYR7tUR_QCCPS-j8BRPq7tPAhjZqh2fD-kYKc72h%2BB_2Z0RQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1487907621.1327855.1674725111818%40mail.yahoo.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANKYR7tJdhQOR4aud6MWGqznhh7E7UTYQi0jwC%3DK54yBjOk2vg%40mail.gmail.com.
Comments