Friday, January 27, 2023

[MW:33967] Re: IBR Welding Requirements

IBR Regulation 608 onwards specifies  about Welder Qualification certificate.
There is chapter related to  :
QUALIFICATION TESTS FOR WELDERS ENGAGED IN WELDING OF BOILERS AND STEAM-PIPES UNDER CONSTRUCTION, ERECTION AND FABRICATION AT SITE IN INDIA AND IN REPAIRING BOILERS AND STEAM-PIPES BY WELDING

WPS PQR are not required.
Thanks and regards

Vishwas 
IWE 

On Thursday, January 26, 2023 at 2:42:13 PM UTC+5:30 Anand Elankumaran wrote:
Dear Experts,

Could you please provide the details about the IBR Welding requirements in terms of WPS & PQR, WQT.

--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a9be3b62-05c9-47d2-9f83-9a59a27c2e1fn%40googlegroups.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...