[MW:33959] Re: MANDATORY HARDNESS TEST AFTER PWHT

It is depending on Design Construction code / Client specification
Normally ASME  SEC I , piping,  equipment does not call  for Hardness test .
As a practice , random hardness checks are  carried out to ensure effective PWHT.
Maximum Hardness reading shall not exceed 275 - 280 BHN .
Hardness checking procedure shall outline Testing Method, type of equipment, Operator 

API 938 , does specify Hardness of 250 BHN maximum .

Regards

Vishwas - IWE
International Welding Engineer 

 
On Wednesday, January 18, 2023 at 1:18:58 PM UTC+5:30 MACARIO PALOLA wrote:
Sirs,

Is it mandatory to perform hardness test after pwht of P91?
Do we have supporting code?

Thank you for your reply.


Mac

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/27261a7b-c2d3-4abc-ba87-5b830db7d88fn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...