Dear chintan
Ignore my previous reply.
1.if nozzle is fitup like seton and bevel in only seton nozzle not in branch(pipe,plate) than governing thickness will be seton on noozle not branch(pipe,plate).
Reason- welding to be done around seton nozzle with whatever fillet require.
2. If noozle is fitup like seton and bevel in only branch(plate,pipe) than governing thickness will branch thickness
Reason- in this case welding to be filled in bevel of branch so branch thickness will be the mandatory thickness for wps.
3.if noozle and branch both has bevel and seton noozle fitup on branch than whichever is maximum thickness will be mandatory thickness
On Thu, 5 Jan 2023, 12:53 pm Chintan Raval, <chintan51@gmail.com> wrote:
Dear Expert,--Kindly advice,For Pressure Vessel as per ASME Sec 8 Div 1,Nozzle to Shell full penetration weld of Set on type nozzle, which is the governing thickness for wps selection i.e. thickness of nozzle or thickness of shell or both.In a typical case,Nozzle thickness 14 mm, needs to be welded on another nozzle of thickness 250 mm.WPs available is with 5 mm to 200 mm range.Is this wps can be used for set on type nozzle as it cover range of nozzle thickness
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS43ZLNQgO-s0Am8pQw5bJHg2X8SZBSTaZJXTy0zytLymFA%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k9E_bRx3y566Y3HXf%2BLuwbU6T_a7C0QnbYfj%3DUFuF5YAQ%40mail.gmail.com.
Comments