[MW:33955] Re: Unequal wall thickness same base metel

Asme 31.4 mention 2.38 maimum

On Mon, 23 Jan 2023, 18:57 Karunakaran Karan, <karunaqc@gmail.com> wrote:
Dears, 
    Clarify same base metal but different  wall thickness(11.97 and 7.9mm)please any tolerance for fitup and standard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw_1xCz9wB1pjpuCRWSdejNko%3DAaKaVBE6GXjTz1CC9OUQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS